Retrofitting of Concrete Structures for Shear and Flexure with Fiber-Reinforced Polymers

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Retrofitting of Concrete Structures for Shear and Flexure with Fiber-Reinforced Polymers

Author(s): Shamim A. Sheikh, David DeRose, and Jamil Mardukhi

Publication: Structural Journal

Volume: 99

Issue: 4

Appears on pages(s): 451-459

Keywords: fibers; flexure; polymer; shear

DOI: 10.14359/12114

Date: 7/1/2002

Abstract:
Damage sustained by foundation walls and large beams in a building was simulated in full-size to near-full-scale model specimens in the laboratory. The damaged specimens were repaired with carbon and glass fiber-reinforced polymer (CFRP and GFRP) sheets and wraps, and tested to failure. Companion control specimens were also tested to failure without rehabilitation to provide a basis for comparison and evaluate the effectiveness of the repair techniques. Test results showed that fiber-reinforced polymers (FRPs) were effective in strengthening for flexure as well as shear. Over-reinforcing in flexure resulted in shifting the failure to shear mode, which in some cases may be undesirable. Strengthening of a member in shear, on the other hand, resulted in increasing the ultimate displacement by more than tenfold, and toughness by a factor of more than 26. Available analytical procedures and building code provisions were found to simulate the behavior of specimens retrofitted with FRP reasonably well.