Precast Reinforced Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Precast Reinforced Concrete Structures

Author(s): C. D. Wailes, Jr.

Publication: Journal Proceedings

Volume: 46

Issue: 6

Appears on pages(s): 841-855

Keywords: no keywords

DOI: 10.14359/12100

Date: 6/1/1950

Abstract:
Several examples of the use of precast concrete in industrial, commercial and residential structures are described. Special design considerations, manufacturing methods, erection techniques and the inspection and testing of precast members are discussed.