Title: Effects of High-Velocity Water oin Bonneville Dam Concrete

Author(s): R. R. Clark

Publication: Journal Proceedings

Volume: 46

Issue: 6

Appears on pages(s): 821-839

Keywords: no keywords

DOI: 10.14359/12099

Date: 6/1/1950

Abstract:
The author compares the progressive erosion which has taken place in the stilling basin of Bonneville Dam with that anticipated in the design, together with the repairs that have been made and the effect on the repairs of the action of high-velocity water.