Design and Construction of Joints in Concrete Pavements with a supplement on Sturctural Design of Joints for Airport Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design and Construction of Joints in Concrete Pavements with a supplement on Sturctural Design of Joints for Airport Pavements

Author(s): Willian Van Breemen, E. A. Finney, and Thomas B. Pringle

Publication: Journal Proceedings

Volume: 46

Issue: 6

Appears on pages(s): 789-819

Keywords: no keywords

DOI: 10.14359/12098

Date: 6/1/1950

Abstract:
The basic fundamental conditions involved in the design and construction of joints are discussed. Various types of joints and load transfer devices are described, as well as various forms of structural failure of joints. Reccomendations are given for the design, fabrication and installation of load-transfer devices, the construction and finishing of the concrete surrounding the joint assembly and the sealing of joints. A supplement disusses joints for heavy duty airport pavements.