Title: Effect of Sustained Loading on Compressive Strength and Modulus of Elasticity of Concrete

Author(s): George W. Washa and Paul G. Fluck

Publication: Journal Proceedings

Volume: 46

Issue: 5

Appears on pages(s): 693-700

Keywords: no keywords

DOI: 10.14359/12089

Date: 5/1/1950

Abstract:
This paper presents results which show the plastic flow characteristics of hand-rodded and vibrated concrete over a 10 1/2-year period. Three different cements and three different water-cement ratios were included in the test program. The effect of the 10 1/2-year loading period on the compressive strength and the modulus of elasticity is also shown.