The Problem of Slab Dimensions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Problem of Slab Dimensions

Author(s): Subcommittee II, ACI Committee 325

Publication: Journal Proceedings

Volume: 46

Issue: 4

Appears on pages(s): 641-648

Keywords: no keywords

DOI: 10.14359/12084

Date: 4/1/1950

Abstract:
The dimensions of concrete pavement slabs necessary for optimum results depnd on and are influenced by a great many factors, economic as well as physical. The factors and their relationship to slab dimensions discussed include strength, elstic and plastic properties, volume change, sungrades, construction conditions and slab thickness, length and width.