Abstract:
From the viewpoint of an architect, inspection on a job involving architectural and structural concrete encompasses a number of factors. Accurate plans and specifications, testing and developing the concrete mix design, proper erection of forms and placement of concrete, and systematic curing require close attention by a competent superintendent and qualified inspectors.