Design and Construction of a Circulating Water Intake

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design and Construction of a Circulating Water Intake

Author(s): W. S. Colby

Publication: Journal Proceedings

Volume: 46

Issue: 3

Appears on pages(s): 497-508

Keywords: no keywords

DOI: 10.14359/12070

Date: 3/1/1950

Abstract:
The author describes the design and construction of a 250,000 gpm power plant intake, An interesting feature of the ppump well cofferdam was the reinforced concrete ring wales, which resulted in savings in operations becasuse the interior of the cofferdam was kept clear for excavating, driving of drilled-in cassions, tremie operations and placing of the pump well concrete.