Volume Changes in Small Concrete Cylinders During Freezing and Thawing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Volume Changes in Small Concrete Cylinders During Freezing and Thawing

Author(s): Rudolph C. Valore

Publication: Journal Proceedings

Volume: 46

Issue: 2

Appears on pages(s): 417-434

Keywords: no keywords

DOI: 10.14359/12065

Date: 2/1/1950

Abstract:
The volume-temperature behavior of small concrete cylinders was observed, using a new mercury-displacement dilatometer, during freezing and thawing cycles in which the range 40 to -20 F was traversed at various rates. Specimens cast from a mix containing 6 bags of portland cement per cu yd, plain and modified by the addition of an air-entraining agent, were tested in air-dry, vacumn-saturated and partially saturated conditions. Volume-temperature relationships for sir-dry specimens yielded uniform thermal expansion data, but those for vacumn-saturated specimens showed departures in the form of transient expansions during freezing, and residual expansions for following thawing of about 0.8 and 0.4 percent, respectively; a single slow cycle produced decreases in dynamic E exceeding 60 percent. Much smaller departures were observed for partially saturated specimens (65 to 85 percent of vacumn-saturation) and included, in addition to transient and residual expansions, secondary effects of freezing termed "shrinkage" and relaxation phenomena. The magnitude of the transient and residual expansions appeared to depend upon the rate of cooling and heating, the degree of saturation of the specimen and, during the slow cycle, upon the degree of supercooling before freezing.