A Shortcut for Determining Reinforcement in Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Shortcut for Determining Reinforcement in Reinforced Concrete

Author(s): V. Bogvad-Christensen

Publication: Journal Proceedings

Volume: 46

Issue: 12

Appears on pages(s): 285-291

Keywords: no keywords

DOI: 10.14359/12058

Date: 12/1/1949

Abstract:
This paper presents a graph which gives the complete relationship between moments, thrusts, concrete dimensions, reinforcement and resulting stresses for the reinforced concrete members in question.