Suggestions on Concrete Floor Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Suggestions on Concrete Floor Construction

Author(s): Ernst Gruenwald

Publication: Journal Proceedings

Volume: 46

Issue: 9

Appears on pages(s): 49-54

Keywords: no keywords

DOI: 10.14359/12043

Date: 9/1/1949

Abstract:
The relationship between good concrete floors and the proper selection of cement and aggregates is discussed. Data are cited to emphasize the advantage of coarse-aggregate mixes over cement-sand topping for concrete floors.