Air Replaces Sand in "No-Fines" Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Air Replaces Sand in "No-Fines" Concrete

Author(s): Rudolph C. Valore, Jr. and William C. Green

Publication: Journal Proceedings

Volume: 47

Issue: 6

Appears on pages(s): 833-846

Keywords: no keywords

DOI: 10.14359/12038

Date: 6/1/1951

Abstract:
Concretes containing high-early strength cement, 20 to 30 percent entrained air in place of fine aggregate, siliceous pea gravel and a proprietary resin or detergent air-entraining agent, were made using ordinary rotating tilt-drum mixers. The maximum air contents in mixes having a compressive strength of 500 psi (28 days) were 25 percent (3.3 bag mix) and 29 percent (5.6 bag mix). The ratio of compressive to transverse and bond strengths was about 3. The saturation coeffcient and capillarity were much lower, the resistance to freezing and thawing generally higher, and the thermal conductivity (k) 30 to 40 percent lower than for nonaerated sand-gravel concrete. The drying shrinkage was about the same as for nonaerated concrete. The compressive strength of all mixes decreased about 100 psi for each percent increase in air content, which was difficult to control.