Title: Blade Changes Improve Tilting Mixer

Author(s): Glenway Maxon

Publication: Journal Proceedings

Volume: 47

Issue: 12

Appears on pages(s): 297-300

Keywords: no keywords

DOI: 10.14359/11992

Date: 12/1/1950

Abstract:
Recent experiments as well as earlier studies on changing the blading of tilting concrete mixers so as to improve the quality of the mixed concrete are described. The evolution of the blade shapes and the effect of these changes on the path of the materials through the mixer are illustrated.