Water-Solublity of Alkalies in Portland Cement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Water-Solublity of Alkalies in Portland Cement

Author(s): J. L. Gilliland and T. R. Bartley

Publication: Journal Proceedings

Volume: 47

Issue: 10

Appears on pages(s): 153-160

Keywords: no keywords

DOI: 10.14359/11982

Date: 10/1/1950

Abstract:
In an effort to show correlation of soluble alkalies with alkali-aggregate reaction, the authors hydrate a number of cement for periods up to 90 days and analyzed water extracts of the ground, hydrated cement. However, the correlation with expansions of mortar bars prepared with reactive aggregate was not improved by considering water-soluble alkalies rather than total alkalies. The rate at which the alkalies become water-soluble in hydrating cement indicates that the alkali-bearing phases in cement hydrate quite readily.