Tests of Paper Molds for Concrete Cylinders

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tests of Paper Molds for Concrete Cylinders

Author(s): Robert A. Burmeister

Publication: Journal Proceedings

Volume: 47

Issue: 9

Appears on pages(s): 17-24

Keywords: no keywords

DOI: 10.14359/11963

Date: 9/1/1950

Abstract:
Concrete test cylinders cast in a new type paper mold had a compressive strength lower than that predicted for the concrete mix used. Investigation showed that cracks and mechanical injuries to the outer shell of the concrete cylinder caused by movement of the paper stock during the first 24 hours of curing reduced the strength of the cylinder. To a lesser degree this was true also of the paraffined paper molds in common use for casting test cylinders, specimens cast in both types of paper molds showing lower strengths than test cylinders from the same mix cast in steel molds.