On Evaluation of Rotation Capacity for Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: On Evaluation of Rotation Capacity for Reinforced Concrete Beams

Author(s): Pier Giorgio Debernardi and Maurizio Taliano

Publication: Structural Journal

Volume: 99

Issue: 3

Appears on pages(s): 360-368

Keywords: capacity; curvature; reinforced concrete.

DOI: 10.14359/11920

Date: 5/1/2002

Abstract:
In the nonlinear analysis of reinforced concrete (RC) structures, the behavior in the plastic range has a notable importance. The modeling, however, is very complex and depends on many factors. Furthermore, the experimental results are rather scattered. This paper presents a simplified procedure that, on the basis of a wide experimental investigation on RC beams and with some hypotheses confirmed in literature, takes into account the aspects that emerged in the experimental investigation and which significantly influence the structural behavior, and in particular, the curvature: the influence of the height of the compression zone on the ultimate concrete strain; the tension-stiffening in the plastic range; and the influence of shear on the extension of plastic zone. Integration of the mean curvatures along the beams yields plastic rotation values that are in good agreement with the experimental results. In particular, as confirmed by other researchers, a size effect on the rotation capacity is observed: it leads to a diminution of the plastic rotation with an increase of the height of the beams which have the same percentage of tensile reinforcement.