Coral and Salt Water as Concrete Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Coral and Salt Water as Concrete Materials

Author(s): John G. Dempsey

Publication: Journal Proceedings

Volume: 48

Issue: 10

Appears on pages(s): 157-166

Keywords: no keywords

DOI: 10.14359/11877

Date: 10/1/1951

Abstract:
Concrete in which coral and its related soft and porous limestones are used as aggregate presents more than the usual number of problems in controlling uniformity and quality. Using sea water for mixing has always been a reluctant last resort. This paper describes coral materials, the problems arising from their use, and the methods of mix control used to btain uniformly satisfactory concrete. Notes on the action of sea water are presented with an account of field experience with it.