Manufacture and Use of Machine-Made Precast Structural Elements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Manufacture and Use of Machine-Made Precast Structural Elements

Author(s): A. G. Streblow

Publication: Journal Proceedings

Volume: 48

Issue: 10

Appears on pages(s): 125-132

Keywords: no keywords

DOI: 10.14359/11874

Date: 10/1/1951

Abstract:
Experience with precast piles, joists and cored roof and floor sections and the introduction of automatic block making machines suggest the development of new precast products. The characteristics and application of floor and roof slabs, wall sections, prefabricated packaged buildings, columns, beams, planks and special structures are described.