Title: Vibration Practices in Pipe, Precast, and Block Manufacture

Author(s): George W. Washa

Publication: Journal Proceedings

Volume: 49

Issue: 6

Appears on pages(s): 945-952

Keywords: no keywords

DOI: 10.14359/11865

Date: 6/1/1953

Abstract:
The discussion of this broad topic is confined to statements regarding present practices. No attempt has been made in this highly competitve and controversial field to indicate superioirty of one method or process over another. Obviously it has not been possible to describe all prcesses in use at the present time.