Title: Application of Vibration to Concrete Pavement Construction

Author(s): A. G. Timms

Publication: Journal Proceedings

Volume: 49

Issue: 6

Appears on pages(s): 933-942

Keywords: no keywords

DOI: 10.14359/11864

Date: 6/1/1953

Abstract:
Brief description and summary of tests and experience in the United States and Europe in vibrating pavement concrete. Effect of vibration on tolerances in composition of the fresh concrete, gradation of coarse aggregate, and maintaining line and grade of forms are factors in the development of adaquate vibration equipment.