Vibration of Mass Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Vibration of Mass Concrete

Author(s): Lewis H. Tuthill

Publication: Journal Proceedings

Volume: 49

Issue: 6

Appears on pages(s): 921-931

Keywords: no keywords

DOI: 10.14359/11863

Date: 6/1/1953

Abstract:
Vibration has already done much to improve the quality of mass concrete. It has completely changed our concept of what is practical and desirable as a mass-concrete mix. Together with air entrainment it has made mixes of very low cement content placable with reductions in unit water content up to 80 lb percu yd. O ther improvements in quality or in cost, or both, can result when full advantage of vibration is taken to place mixes with larger aggregate in many cases where there is reinforcing, to place concrete in thicker layers, to permit useof larger buckets, and to eliminate poor bond at cold joints.