Title: Guide for the Use of Preplaced Aggregate Concrete for Structural and Mass Concrete Applications

Author(s): ACI Committee 304

Publication: Materials Journal

Volume: 88

Issue: 6

Appears on pages(s): 650-668

Keywords: fluidizing; heavyweight concretes; preplaced aggregate concrete; inserts; grout; underwater construction; Materials Research

DOI: 10.14359/1186

Date: 11/1/1992

Abstract:
The preplaced-aggregate (PA) method for concrete construction is explained, special properties are described, and materials requirements are given where they differ from those used in normal concrete. A brief history of the development of the procedure is covered. Short descriptions of several typical applications are included.