Bracing Walls for Multistory Buildings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bracing Walls for Multistory Buildings

Author(s): Norman B. Green

Publication: Journal Proceedings

Volume: 49

Issue: 11

Appears on pages(s): 233-248

Keywords: no keywords

DOI: 10.14359/11816

Date: 11/1/1952

Abstract:
Methods are developed for the stress analysis and design of the multistory reinforced concrete bracing wall, by treating it as a special type of beam and column frame having relatively wide members. Elastic requirements for a bracing wall are established. There is a discussion of the general problem of lateral load distribution to bracing walls and an intirely new method of distribution is presented, which equalizes wall deflections.