Effect of Time of Application of Sealing Compund on the Quality of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Time of Application of Sealing Compund on the Quality of Concrete

Author(s): G. E. Burnett and M. R. Spindler

Publication: Journal Proceedings

Volume: 49

Issue: 11

Appears on pages(s): 193-200

Keywords: no keywords

DOI: 10.14359/11812

Date: 11/1/1952

Abstract:
Laboratory experiments with mortar specimens indicate an advantage for applying curing compund to unformed concrete at approximately the time of set. Loss of mixing water from evaporation up to this point is shown to be beneficial to strength and brasion resistance. Subsequent loss is shown to be detremental. The benefit from loss of water before set appears to be directly related to the decrease in water-cement ratio.