Title: Proposed Revision of Minimum Standard Requirements for Precast Concrete Floor Units (ACI 711-46)

Author(s): ACI Committee 711

Publication: Journal Proceedings

Volume: 49

Issue: 11

Appears on pages(s): 169-184

Keywords: no keywords

DOI: 10.14359/11810

Date: 11/1/1952

Abstract:
Proposes to change the existing Standard by adding descriptions of assembled concrete block, precast inverted T-beam joist with precast filler block, and inverted precast slab and T-joist types of floor units. New information is incorporated on moment bar spacing, steel requirements, distance between lateral supports, and provisions for tests. References for the ACI Building Code are brought up to date and the Appendix excerpts are taken from the 1951 Building Code. Minor editorial changes are made to clarify some of the other sections.