Title: Heavy Duty Concrete Floors

Author(s): E. E. Eckert

Publication: Journal Proceedings

Volume: 49

Issue: 10

Appears on pages(s): 109-116

Keywords: no keywords

DOI: 10.14359/11807

Date: 10/1/1952

Abstract:
Brief but specific directions for mixing, placing, finishing, and curing concrete for heavy duty concrete floors. Emphasis is on the careful control of mixing water, and the selection, handling, and use of a tough durable aggregate. Precautions are given for avoiding subsequent failure.