Title: Crushed Stone Production

Author(s): A. T. Goldbeck

Publication: Journal Proceedings

Volume: 50

Issue: 5

Appears on pages(s): 761-772

Keywords: no keywords

DOI: 10.14359/11793

Date: 5/1/1954

Abstract:
Prospecting for and production of commercial crushed stone are detailed with emphasis on modern trends in the crushed stone industry. Quarrying, transportantion og quarried stone, crushing, screening, washing, production of stone sand, and related operations are described as to equipment, methods, and trends. A selected bibliography of 71 references completes the report.