Strap Steel for Prestressed Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strap Steel for Prestressed Concrete Structures

Author(s): K. P. Milbradt

Publication: Journal Proceedings

Volume: 50

Issue: 1

Appears on pages(s): 357-363

Keywords: no keywords

DOI: 10.14359/11768

Date: 1/1/1954

Abstract:
A new type of prestressing steel - strap steel - is introduced as offering possible economy for this type of construction. Tempered spring steel, 0.048 x 0.625 in., having an average ultimate strength of 215,000 psi and a yield strength of 182,000 psi were used. Economical prestressing clamps were developed. This type of prestressing was then applied to a test beam. Specific conclusions from the test were: (1) the strap was easily handled, placed, clamped, and stressed either singly or mutiply in one operation; (2) bond was sufficient to transfer the prestressing force; and (3) ultimate load deflection for the test beam was obtained with little elongation of the steel.