Limit Analysis and Design

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Limit Analysis and Design

Author(s): William Prager

Publication: Journal Proceedings

Volume: 50

Issue: 12

Appears on pages(s): 297-304

Keywords: no keywords

DOI: 10.14359/11763

Date: 12/1/1953

Abstract:
Many problems concerning limit analysis and limit design of reinforced concrete beams and frames can be treated geometrically in terms of the safe domain in load space. The procedure is illustrated by a typical example involving a frame.