Pier 57 Concreted Through the Winter

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pier 57 Concreted Through the Winter

Author(s): M. D. Morris

Publication: Journal Proceedings

Volume: 50

Issue: 12

Appears on pages(s): 281-284

Keywords: no keywords

DOI: 10.14359/11761

Date: 12/1/1953

Abstract:
Although much has been written about New York's Pier 57 and the new techniques used in its construction, little has been said about the fact that through the five months from November, 1951, through March, 1952, regardless of near zero temperatures, concrete was placed at 60 F and steam cured with no loss of time or ultimate strength. This brief description of this work is not posed as a standard text on the subject of winter concreting but is submitted as a record of how one job was done sucessfully.