Concrete for Radiation Shielding

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete for Radiation Shielding

Author(s): Edwin J. Callan

Publication: Journal Proceedings

Volume: 50

Issue: 9

Appears on pages(s): 17-44

Keywords: no keywords

DOI: 10.14359/11733

Date: 9/1/1953

Abstract:
Concrete for shielding nuclear radiation is discussed, with emphasis on factors relating to concrete technology and cost. The types of radiation and mechanics of radiation shielding are presented briefly, and data regarding concrete for shielding are reviewed. Tables and curves of concrete thickness required for shielding are given for bothordinary and heavy concrete. Problems involved in the use of special concrete are discussed. An outline of a procedure for designing concrete shielding is presented.