Strength of Continuous Prestressed Concrete Beams Under Static and Repeated Loads

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength of Continuous Prestressed Concrete Beams Under Static and Repeated Loads

Author(s): T. Y. Lin

Publication: Journal Proceedings

Volume: 51

Issue: 6

Appears on pages(s): 1037-1059

Keywords: no keywords

DOI: 10.14359/11731

Date: 6/1/1955

Abstract:
Basic principles underlying the behavior of statically indeterminate prestressed concrete structures were investigated by testing four continuous beams, each 50 ft long. The cracking and ultimate strengths of these beams were measured and evaluated for static loads as well as for repeated loads up to 5,000,OOO cycles. Beam reactions, deflections, and strains were recorded for analysis. The effects of adding nonprestressed mild steel reinforcement were studied.