Title: Precast Prestressed Lightweight Concrete Construction

Author(s): Arthur M. James

Publication: Journal Proceedings

Volume: 51

Issue: 6

Appears on pages(s): 1025-1034

Keywords: no keywords

DOI: 10.14359/11730

Date: 6/1/1955

Abstract:
Design, fabrication, and erection of precast and prestressed floor and roof beams and slabs of lightweight expanded shale concrete are described. A discussion of the lastic modulus of expanded shale concrete is based on measured camber at prestressing. Cost data on the beams and slabs and a yard test of one prestressed beam are included.