Ball Test for Field Control of Concrete Consistency

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ball Test for Field Control of Concrete Consistency

Author(s): J. W. Kelly and Milos Polivka

Publication: Journal Proceedings

Volume: 51

Issue: 5

Appears on pages(s): 881-888

Keywords: no keywords

DOI: 10.14359/11722

Date: 5/1/1955

Abstract:
A simple field test is described for determining the consistancy of fresh concrete interms of the penetration of a 6-in. 30-lb ball. Experiences of users are given, and comparisons with slump are made. Considerations in the practical use of the ball are discussed.