Theory of Secondary Arch

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Theory of Secondary Arch

Author(s): B. F. Jakobsen

Publication: Journal Proceedings

Volume: 51

Issue: 4

Appears on pages(s): 741-756

Keywords: no keywords

DOI: 10.14359/11701

Date: 4/1/1955

Abstract:
For circular archs having a ratio of thickness to mean radius greater than 0.3, a central angle less than 100 deg, and under normal loads, high tensile stresses are indicated both at the crown and at the abutments by the usual formulas. A method of computation is proposed which assumes that the stress distribution is linear on radical sections and that the part of the arch not subject to compression may be disregarded.