Magnetite Iron Ore Concrete for Nuclear Shielding

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Magnetite Iron Ore Concrete for Nuclear Shielding

Author(s): J. O. Henrie

Publication: Journal Proceedings

Volume: 51

Issue: 2

Appears on pages(s): 541-550

Keywords: no keywords

DOI: 10.14359/11694

Date: 2/1/1955

Abstract:
Discusses crushing and handling of the magnetite iron ore, which was used as the aggregate for a dense shielding concrete, and the physical properties and costs of magnetite ore concrete are compared to those of other concretes. The mix used had a compressive strength of 4000 psi in 10 days. The methods used in fabricating shielding block are described. Recommendations for pro-ducing a low cost, relatively high density shielding concrete are made. T h e shielding block used (9 x 9 x 18 in. nominal) had a density of 3.7 g per sq cm or 230 lb per cu ft and cost $163.50 per cu yd. The dimensions of the block were quite uniform, having a standard deviation of approximately 0.015 in.