Design and Construction of a Folded Plate Roof Structure

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design and Construction of a Folded Plate Roof Structure

Author(s): Milo S. Ketchum

Publication: Journal Proceedings

Volume: 51

Issue: 1

Appears on pages(s): 449-456

Keywords: no keywords

DOI: 10.14359/11688

Date: 1/1/1955

Abstract:
The H. W. Moore Equipment Co. building, a reinforced concrete structure in Denver, Colo., utilized two types of folded plate shells: a discontinuous Z-shaped shell arranged to provide a north light clerestory, and a continuous series of inverted V-shapes. The latter shell was designed to carry two 15-ton cranes on the roof system. The analysis of stresses made use of the latest refinements involving the effect of deflection on the transverse stresses in the slabs. The roof plates were constructed with both conventional and movable forms, and some structural elements were precast on the ground and raised into place.