Observations on the Resistance of Concrete to Freezing and Thawing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Observations on the Resistance of Concrete to Freezing and Thawing

Author(s): Hubert Woods

Publication: Journal Proceedings

Volume: 51

Issue: 12

Appears on pages(s): 345-350

Keywords: no keywords

DOI: 10.14359/11682

Date: 12/1/1954

Abstract:
A survey and analysis of the more important investigations on freezing and thawing of concrete show that significant general conclusions can be drawn. Some of these conclusions can be presnted in a manner designed to show their reasonableness, but without detailed evidence.