Mixing Water Control by Use of a Moisture Meter

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mixing Water Control by Use of a Moisture Meter

Author(s): C. B. Van Alstine

Publication: Journal Proceedings

Volume: 52

Issue: 11

Appears on pages(s): 341-347

Keywords: no keywords

DOI: 10.14359/11604

Date: 11/1/1955

Abstract:
Conditions at Reservoir No. 22 Dam created severe fluctuations of free moisture in sand and pea gravel. Use of a moisture meter as a basis for ad-justments in water is described. Charts show the effectiveness of the device, in conjunction with other control measures, as an aid to producing quality concrete.