Tests of Anchors for Mass-Concrete Forms

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tests of Anchors for Mass-Concrete Forms

Author(s): Thomas B. Kennedy and Walter O. Crawley

Publication: Journal Proceedings

Volume: 52

Issue: 10

Appears on pages(s): 139-147

Keywords: no keywords

DOI: 10.14359/11592

Date: 10/1/1955

Abstract:
The tests covered in this paper were intended to determine the holding strength of several designs of anchors for securing cantilever forms to mass roncrete surfaces. The investigation consisted of the fabrication of four blocks of low-strength, 6-in. aggregate concrete in which a total of 48 anchors wxc embedded and tested at ages ranging from 24 to 72 hr. The results in-dicate that, under the test conditions used, adequate holding strength was dc-veloped in practically every case by the time the concrete was 3 days old.