Shell Reinforcement Not Parallel to Principal Stresses

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shell Reinforcement Not Parallel to Principal Stresses

Author(s): Emilio Rosenblueth

Publication: Journal Proceedings

Volume: 52

Issue: 9

Appears on pages(s): 61-71

Keywords: no keywords

DOI: 10.14359/11586

Date: 9/1/1955

Abstract:
Current methods of shell design implicitly assume that concrete can take tension. In intermediate steps those methods strive to satisfy strain relation-ships. The procedure developed herein consistently assigns no tension to the concrete and only takes into account considerations of equilibrium, not strain relationships. The procedure requires the addition and subtraction of stress tensors, which is greatly simplified through the use of Mohr’s diagram. It is applicable only to states of pure axial or "membrane" stresses.