Mechanisms of Alkali-Aggregate Reaction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanisms of Alkali-Aggregate Reaction

Author(s): Robert G. Pike, Donald Hubbard, and Herbert Insley

Publication: Journal Proceedings

Volume: 52

Issue: 9

Appears on pages(s): 13-34

Keywords: no keywords

DOI: 10.14359/11583

Date: 9/1/1955

Abstract:
An interferometer procedure was used to determine the attack on character-istic active and nonreactive aggregates over an extended pH range, in solutions of NaOH, Ca (OH),, NaOH + Ca (OH), and in aqueous extracts of high-and low-alkali cements. Curves are given showing the hygroscopicity of high- and low-alkali cement pastes and powders and the same cements with added reactive and nonreactive aggregates. Curves are given showing ex-pansion of the mortar bars containing various percentages of Pyrex glass of different grain sizes. Microscopic studies of reactive aggregates in high-alkali cements are described, and photographs show instances where the major reaction takes place inside the opal grain rather than at the outside of the particle. This effect is rationalized in terms of the uneven distribution of the migratable ions. An expansion of 300 percent is demonstrated when opal reacts with soda to form a sodium silicate hydrate complex. It is believed that this expansion is the major cause of alkali-aggregate distress in concrete.