Oldest Concrete Street in the United States

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Oldest Concrete Street in the United States

Author(s): Luke M. Snell and Billie G. Snell

Publication: Concrete International

Volume: 24

Issue: 3

Appears on pages(s): 72-74

Keywords:

DOI:

Date: 3/1/2002

Abstract:
Bellefontaine, Ohio, is home to the United States’ first concrete street. In 1891, as an experiment to improve street conditions, the city council hired George Bartholomew to provide the concrete for an 8-ft segment of pavement, which was designed by James C. Wonders. After this experiment proved successful, the square surrounding the courthouse was also paved , creating the first concrete street. The street is still open to light traffic today with a statue of Bartholomew at one end to prevent trucks from damaging the pavement. .