Tables for Circularly Curved Horizontal Beams with Symmetrical Uniform Loads

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tables for Circularly Curved Horizontal Beams with Symmetrical Uniform Loads

Author(s): Martin Schulz and Mauricio Chedraui

Publication: Journal Proceedings

Volume: 53

Issue: 5

Appears on pages(s): 1033-1040

Keywords: no keywords

DOI: 10.14359/11569

Date: 5/1/1957

Abstract:
These tables will simplify and expedite the engineer's task of calculating cir-cular beams without developing the formulas. Step-by-step derivation of the tables is given.