Hot Weather Concreting Problems

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Hot Weather Concreting Problems

Author(s): ACI Committee 605

Publication: Journal Proceedings

Volume: 53

Issue: 5

Appears on pages(s): 1025-1032

Keywords: no keywords

DOI: 10.14359/11568

Date: 5/1/1957

Abstract:
This progress report discusses the subject matter which is proposed for inclusion in a recommended practice now being drafted by the committee. It discusses, briefly, effects of concreting in hot weather; factors in minimizing hot weather difficulties; keeping concrete temperature down by controlling the temperature of its ingredients; production and delivery, placement and protection, and concrete testing in hot weather.