Bond between Near-Surface Mounted Fiber-Reinforced Polymer Rods and Concrete in Structural Strengthening

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bond between Near-Surface Mounted Fiber-Reinforced Polymer Rods and Concrete in Structural Strengthening

Author(s): Laura De Lorenzis and Antonio Nanni

Publication: Structural Journal

Volume: 99

Issue: 2

Appears on pages(s): 123-132

Keywords: bond; concrete; polymer; rod; slip

DOI: 10.14359/11534

Date: 3/1/2002

Abstract:
The use of near-surface mounted (NSM) fiber-reinforced polymer (FRP) rods is a promising technology for increasing flexural and shear strength of reinforced concrete (RC) members. As this technology emerges, the structural behavior of RC elements strengthened with NSM FRP rods needs to be fully characterized, and bond is the first issue to be addressed. Bond is of primary importance since it is the means for the transfer of stress between the concrete and the FRP reinforcement to develop composite action. The objective of this research program was to investigate bond between NSM FRP rods and concrete. Some of the factors expected to affect bond performance were addressed, namely: bonded length, diameter and surface configuration of the rod, type of FRP material, and size of the groove in which the rod is embedded. Results are presented and discussed in this paper.