Proposed Recommended Practice for Compression Test Results of Evaluation of Field Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Recommended Practice for Compression Test Results of Evaluation of Field Concrete

Author(s): ACI Committee 214

Publication: Journal Proceedings

Volume: 53

Issue: 12

Appears on pages(s): 561-579

Keywords: no keywords

DOI: 10.14359/11529

Date: 12/1/1956

Abstract:
Statistical methods provide valuable tools for assessing results of strength teats, and such information is also of value in refining design criteria and specifications. The report discusses briefly the numerous variations that occur in the strength of concrete and presents statistical methods which are useful in interpreting these variations. Criteria are offered that can be used to establish specifications and maintain required uniformity.