Particle Interference in Concrete Mixes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Particle Interference in Concrete Mixes

Author(s): B. J. Butcher and H. J. Hopkins

Publication: Journal Proceedings

Volume: 53

Issue: 11

Appears on pages(s): 545-556

Keywords: no keywords

DOI: 10.14359/11528

Date: 11/1/1956

Abstract:
C. A. G. Weymouth’s theory of particle interference postulates that fine particles infiltrate into the voids of larger particles. The authors’ examination of Weymouth’s method of calculation has shown his results to be in conflict with recognized physical laws. They advance a new method of applying the Weymouth criterion for particle interference in concrete mixes, based upon a consideration of the complete grading of solids instead of applying the criterion in turn to each successive size group.