Considerations in the Selection of Slab Dimensions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Considerations in the Selection of Slab Dimensions

Author(s): Subcommittee II, ACI Committee 325

Publication: Journal Proceedings

Volume: 53

Issue: 11

Appears on pages(s): 433-454

Keywords: no keywords

DOI: 10.14359/11523

Date: 11/1/1956

Abstract:
The principal dimensions of a pavement slab are length, width, and thickness. These dimensions and the factors which determine them are discussed separately and typical examples are given of the dctcrminntion of slab thickness for specific sets of conditions.