Shearing Strength of Reinforced Concrete Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shearing Strength of Reinforced Concrete Slabs

Author(s): Richard C. Elstner and Eivind Hognestad

Publication: Journal Proceedings

Volume: 53

Issue: 7

Appears on pages(s): 29-58

Keywords: no keywords

DOI: 10.14359/11501

Date: 7/1/1956

Abstract:
Presented as a research report with out practical design recommendations, this paper reports the methods and results of experimental work on the shearing strength of reinforced concrete slabs subjected to a centrally located, concentrated load. Tests of thirty-nine 6-ft square column slabs are reported.